초록
F.R.P specimens were made by mixture CM(chopped mat)450-104 Matrix & RC(roving clothes)570-100 Roving, the mixture ratio Resin: hardener (92:8)for tensile test. It was also made of plates by hand lay-up method and was been cured for 24 hours and then was cut tensile specimens in accordance with ASTM D638 Type 3. Knowing exact behavior of bonded area's stress and strain when the tensile test was going on, the test specimens were made of 2 plies laminae of F.R.P in each for supporting cut part in middle of specimen length. And in middle part also, were covered of F.R.P plies of 1/2, 2/3 length of specimen in each as well. Also we consider shear stress in adhered area. this study reveals that as plys length is more longer, rupture stress grows remarkably larger.